Effects of dry joints on the compressive behaviour of refractory linings
02 Nov 2011
Kirill Andreev, Sido Sinnema; Tata Steel RD&T IJmuiden, The NetherlandsTo support optimisation of refractory masonry structures compressibility of dry joints of magnesia-carbon and magnesia-chromite bricks have been investigated. Laboratory scale tests, field measurements and finite element modelling have been performed. Measurements done in wide temperature range have shown that the exponential form of the joint closure curve results from gradual closure of initially non parallel surfaces. The stress needed to close the joint was found to be proportional to the material stiffness. Temperature influences the joint closure by changing the stiffness of material and by reducing the initial joint gap due to thermal dilatation.
Paper presented at UNITECR 2011, Kyoto, Japan, October 30 - November 2, 2011